Bulb flat steel LR Grade A| Shipbuilding Flat Bulb steel LR

Come from:United Iron and Steel Limited  Editor:United Iron and stee Access:

Bulb flat steel LR Grade A| Shipbuilding Flat Bulb steel LR A
 
Our Mill produce and export shipbuilding profile, bulb flat, flat bar material LR Grade A, LR Grade B, LR Grade D, LR Grade AH36,LR Grade AH32, LR Grade DH32,LR Grade DH36 for ship building project.
 
Our bulb flat steel mainly size is HP80*5, HP80*6, HP100*7, HP100*8, HP120*6, HP120*7 , HP120*8, HP140*7, HP140*8, HP140*10, HP160*7, HP160*8, HP160*9, HP160*11, HP180*8, HP180*9, HP180*10, HP180*11, HP200*9, HP200*10, HP200*11, HP200*12, HP220*10, HP220*11, HP220*12, HP240*10, HP240*11, HP240*12, HP260*10, HP260*11, HP260*12, HP280*11, HP280*12, HP280*13, HP300*11, HP300*12, HP300*13, HP320*12, HP320*13, HP320*14 and so on
 
 
Our mill shipbuilding bulb flat have passed DNV, ABS , LR , BV, GL , NK, KR, RINA,CCS Approval in quality. The better quality, the most competitive price. if you have any requirement in bulb flat, please feel free to contact us by email sales@unitedsteelplate.com
 
The Chemical or element or Composition LR Grade A bulb flat
 
LR GRADE A bulb flat general Strength Chemical Composition
Grade The Element Max (%)
C Si Mn P S N
LR GRADE A 0.21 0.50 2.5*C 0.035 0.035 0.02
Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
 
 
LR GRADE A  Bulb flat steel  property
Grade   Mechanical Property Charpy V Impact Test
Thickness Yield Tensile Elongation Degree Energy 1 Energy 2
LR GRADE A mm Min Mpa Mpa Min  % 20 J J
t≤50 235 400-520 18% - -
50<t≤70 235 400-520 18% 24 34
70<t≤100 235 400-520 18% 27 41
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal
 
 
The Equivalent of LR Grade A bulb flat for shipbuilding steel profile.
BV Grade A, CCS Grade A, DNV Grade A, GL Grade A, NK Grade A, KR Grade A, RINA Grade A, ABS Grade A