C14200 copper plate|C14200 copper sheet|C14200 DPA

Come from:United Iron and Steel Limited  Editor:United Iron and stee Access:

C14200 copper plate|C14200 copper alloy|C14200 DPA|C14200 Deoxidized Arsenical
 
United iron and steel limited could produce and supply C14200 C14300 C14410 C14415 C14420 C14425 C14500 C14510 C14520 C14530 C14700 C15000 C15100 C15150 C15500 C15650 Copper alloy.
If any need in that material, please contact us by email address: sales@unitedsteelplate.com
 
C14200 Copper alloy usual be used in bus bars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass-to-metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.
 
C14200 Chemical Composition
 
Coppers Nominal Chemical Composition %
Copper Cu(incl Ag) Ag(%)min Ag(Troy oz)min As Sb P Te
C14200 99.4min - - 0.15-0.50 - 0.015-0.040 -
Designation: Phosphorus-Deoxidized Arsenical
Description: DLPS
 
Note: Composition percent maximum unless shown as a range or a minimum
 
1) Includes Cd. Deoxidized with Li or other suitable elements as agreed upon.
(2) Includes Cu + Ag + Sn.
(3) Includes Te + Sn.
(4) Cu + Sum of Named Elements, 99.97% Min.
(5) Includes Co
(6) Includes oxygen-free or deoxidized grades with deoxidizers (such as phosphorus, boron, lithium or others) in an amount agreed upon.
(7) Includes Te + P.
(8) Includes Cu + S + P.
(9) Cu + Sum of Named Elements, 99.9% min.
C14200 Copper supplied Specification:
Coppers
C14200
Hot Rolled Coppers plate Cold Rolled Coppers plate
Thickness mm Width mm Length mm Thickness mm Width mm Length mm
Red Copper 6-15 400-3000 1000-6000 0.2-0.49 300-600 1000-1500
16-20 400-3000 0.5-2.5 600-1000 1000-2500
21-50 600-3000 3-10 600-2500 1000-3000
>10-110 600-1000      
Yellow Brass 6-15 400-2000 1000-6000 0.2-0.49 300-600 1000-1500
16-20 400-2000 0.5-2.5 400-1000 1000-3000
>60 600-2500 3-10 600-2000 1000-2500
Bronze >2.5 600-1000 1000-6000 0.4-0.49 300-500 600-1500
0.5-2.5 500-600 1000-3000
3-10 500-1000 600-2000
Cupronickel >2.5 400-1500 1000-6000 0.5-2.5 300-600 600-1500
3-10 300-1000 600-1500
 


















C14200 Processing and Property:  Excellent hot and cold workability; good forge ability. Fabricated by bending, coining, coppersmith, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.
 
C14200 Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.
 
C14200 Equivalent Grade for Copper alloy
Equivalent Grade for Copper alloy
GB DIN EN ISO UNS JIS
  KRUZZEICHEN NUMBER Symbol Number Symbol Number Number
               
 
 
United iron and steel limited also have stock sizes at our warehouse, if you have requirement in C14200 Copper alloy material; please contact us by email sales@unitedsteelplate.com