Bulb flat steel RINA Grade A|Shipbuilding Flat Bulb RINA A

Come from:United Iron and Steel Limited  Editor:United Iron and stee Access:

Bulb flat steel RINA Grade A| Shipbuilding Flat Bulb steel RINA A
 
Our Mill produce and export shipbuilding profile, bulb flat, flat bar material RINA Grade A, RINA Grade B, RINA Grade D, RINA Grade AH36,RINA Grade AH32, RINA Grade DH32,RINA Grade DH36 for ship building project.
 
Our bulb flat steel mainly size is HP80*5, HP80*6, HP100*7, HP100*8, HP120*6, HP120*7 , HP120*8, HP140*7, HP140*8, HP140*10, HP160*7, HP160*8, HP160*9, HP160*11, HP180*8, HP180*9, HP180*10, HP180*11, HP200*9, HP200*10, HP200*11, HP200*12, HP220*10, HP220*11, HP220*12, HP240*10, HP240*11, HP240*12, HP260*10, HP260*11, HP260*12, HP280*11, HP280*12, HP280*13, HP300*11, HP300*12, HP300*13, HP320*12, HP320*13, HP320*14 and so on
 
 
Our mill shipbuilding bulb flat have passed DNV, ABS , LR , BV, GL , NK, KR, RINA,CCS Approval in quality. The better quality, the most competitive price. if you have any requirement in bulb flat, please feel free to contact us by email sales@unitedsteelplate.com
 
The Chemical or element or Composition RINA Grade A bulb flat
RINA GRADE A bulb flat general Strength Chemical Composition
Grade The Element Max (%)
C Si Mn P S N
RINA GRADE A 0.21 0.50 2.5*C 0.035 0.035 0.02
Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
 
 
RINA GRADE A  Bulb flat steel  property mechanical
Grade   Mechanical Property Charpy V Impact Test
Thickness Yield Tensile Elongation Degree Energy 1 Energy 2
RINA GRADE A mm Min Mpa Mpa Min  % 20 J J
t≤50 235 400-520 18% - -
50<t≤70 235 400-520 18% 24 34
70<t≤100 235 400-520 18% 27 41
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal
 
 
The Equivalent of RINA Grade A bulb flat for shipbuilding steel profile.
BV Grade A, CCS Grade A, DNV Grade A, GL Grade A, NK Grade A, KR Grade A, RINA Grade A, ABS Grade A, LR Grade A